Material Drying
2 views
Agglomeration due to too high drying temperature
Problem Phenomenon
Pellets soften, stick and agglomerate during drying
Cause Analysis
Drying temperature 140C close to softening point 150C
Solution
Lower to 130C and turn the material regularly
Key Takeaway
Drying temperature cannot be close to softening temperature
Was this helpful?
0 people found this helpful