Processing Machinery 4 views

PVDF melt stays too long in the barrel

Problem Phenomenon
The product color becomes darker and degradation occurs
Cause Analysis
Continuous production is interrupted and the material in the barrel is heated for a long time
Solution
Empty the barrel after a 10-minute shutdown, plan reasonably to reduce shutdowns
Key Takeaway
Reducing residence time is a basic principle
PVDFresidence time