Material Drying 2 views

PAR dryer capacity matching

Problem Phenomenon
PAR has strong moisture absorption and long drying time, requiring sufficient dryer capacity.
Cause Analysis
The dryer capacity is insufficient, the hopper residence time is insufficient, and the drying is insufficient.
Solution
The drying hopper capacity meets the material amount for 4-6h; parallel dryers increase throughput.
Key Takeaway
PAR drying capacity matching is essential for continuous production.