Material Analysis
9 views
PBT Products Failing to Reach V-0 Flame Retardant Rating
Problem Phenomenon
In the UL94 flame retardant test, PBT products fail to reach the V-0 rating.
Cause Analysis
The flame retardant formulation is improper or the dosage is insufficient; the product wall thickness is too thin, and heat accumulates quickly during combustion; the flame retardant is unevenly dispersed.
Solution
Optimize the ratio and dosage of the flame retardant (bromine-based + Sb₂O₃ or other combinations); ensure the minimum wall thickness of the product is ≥0.8mm.
Key Takeaway
PBT flame retardancy requires sufficient wall thickness and a reasonable formulation.
Was this helpful?
0 people found this helpful