Material Drying
2 views
Incomplete depolymerization in PET chemical recycling
Problem Phenomenon
The depolymerization process (glycolysis or hydrolysis) in PET chemical recycling is incomplete, and the residual PET amount is too high.
Cause Analysis
Depolymerization temperature is on the low side or time is insufficient; catalyst dosage is insufficient or deactivated; PET and the depolymerizing agent are not fully mixed.
Solution
Increase depolymerization temperature and extend reaction time; optimize catalyst type and dosage; improve stirring and mass transfer efficiency.
Key Takeaway
PET chemical depolymerization efficiency depends on reaction conditions and mass transfer effect.
Was this helpful?
0 people found this helpful