Problem Phenomenon
Local protrusions (ridges) appear on the end face after PET film winding, affecting slitting and use.
Cause Analysis
Local film thickness is too thick, forming ridges; winding tension is uneven; the film slips on the roller surface.
Solution
Improve transverse thickness uniformity (automatic die lip control); optimize the winding tension curve; use nip rollers to improve winding flatness.
Key Takeaway
PET film ridges are a comprehensive manifestation of uneven thickness and poor winding.