Extrusion & Post 2 views

Rubber Migration/Bleeding of acrylonitrile-butadiene-styrene copolymer HIPS Products

Problem Phenomenon
Rubber migration or bleeding appears on the surface of HIPS products, the surface is sticky or discolored, affecting the product appearance and printing performance.
Cause Analysis
(1)The rubber content is too high or the compatibility with the base material is poor (2)The processing temperature is too high, and the rubber partially degrades and migrates (3)The product storage temperature is high, accelerating rubber migration (4)The rubber particle size is too large, making migration easy (5)Additives interact with the rubber to promote migration
Solution
(1)Select a grade with suitable rubber content and compatibility (2)Control the processing temperature within the 220-260°C range (3)The product storage temperature does not exceed 40°C (4)Select a grade with a small rubber particle size (5)Reduce additives that may interact with the rubber
Key Takeaway
HIPS rubber bleeding is caused by compatibility and temperature.