PAI severe screw and barrel wear

Problem Phenomenon
When PAI contains graphite/PTFE/carbon fiber fillers, equipment wear is extremely severe
Cause Analysis
The high filler content and high viscosity of PAI cause abrasive wear and adhesive wear
Solution
Select high wear-resistant bimetallic screw and barrel; regularly check the clearance
Key Takeaway
PAI wear on equipment is all-round
wearbimetallicgraphitePTFEcarbon fiber