Molds & Tooling 2 views

PAI melt mold filling difficulty

Problem Phenomenon
PAI still has very high viscosity and poor flowability in the molten state
Cause Analysis
Viscosity high when processing temperature is below 340°C; mold temperature low
Solution
Increase the melt temperature to 360-380°C; keep the mold temperature high at 200-230°C
Key Takeaway
The temperature and pressure required for PAI processing are second only to PI