Q
PP Jetting Mark
A
Hit the wall first then spread—jetting marks come no more.
Molds & Tooling PP;jetting mark;gate;injection speed;snake-like mark
Q
PP Short Shot
A
PP short shots are mostly a balance problem of speed and venting.
Injection Molding PP;short shot;injection speed;venting;wall thickness
Q
PP Tiger Stripe (Flow Mark)
A
Tiger stripes are flow imprints of rubber phase distribution—stable speed is the core.
Injection Molding PP;tiger stripe;flow mark;injection speed;rubber phase
Q
PP Weak Weld Line Strength
A
PP weld lines must complete entanglement before crystallization.
Molds & Tooling PP;weld line;crystallization;venting;melt temperature
Q
PP Flash
A
For flash of low-viscosity materials, pressure restraint comes first.
Injection Molding PP;flash;low viscosity;injection pressure;clamping force
Q
PP Dimensional Post-shrinkage Drift
A
PP dimensions should be managed by 'post-aging dimension'.
Molds & Tooling PP;post-shrinkage;post-crystallization;dimensional drift;annealing
Q
PP Sink Mark (Shrinkage)
Q
PP '2079851475616104452 Warpage Deformation
A
PP warpage takes 'uniform cooling + sufficient crystallization' as the main direction of attack.
Injection Molding PP;warpage;shrinkage rate;mold temperature;crystallization