Extrusion & Post 11 visualizações

Aramid/Kevlar lamination shows "fuzzy edges"

Fenómeno do problema
Fluffy fiber burrs appear on the cut edges of aramid laminates. This problem is relatively common in lamination molding production and requires comprehensive analysis and solution from multiple aspects of materials, processes, and equipment.
Análise das causas
(1) Process factor: aramid fiber toughness extremely high, conventional tools unable to cut cleanly; this factor affects the '2079851475616104453 and final quality of the product. (2) Material aspect: fluctuations in raw material performance indicators or insufficient pretreatment affect molding quality. (3) Process aspect: control deviations of key process parameters cause the '2079851475616104453 to deviate from optimal conditions. (4) Equipment aspect: equipment precision and maintenance status affect the stable execution of process parameters.
Solução
(1) Material selection: use ultra-sharp carbide or diamond tools specifically for aramid; establish material selection evaluation standards and determine the optimal solution through comparative tests. (2) Implementation measures: use low feed and high rotation speed when cutting; formulate specific operation plans based on actual production conditions and verify implementation effects. (3) Material selection: use shear cutters instead of milling cutters., establish material selection evaluation standards and determine the optimal solution through comparative tests. (4) Preventive measures: establish a sound process control standard and quality inspection system, and regularly review process data for continuous optimization.
Conclusão principal
This problem requires comprehensive analysis from multiple dimensions of materials, processes, equipment, and operation, and should be solved by systematically optimizing process parameters and the quality control system.