Molds & Tooling 3 visualizações

ABS gate 50/60 rule

Fenómeno do problema
ABS gate size 50-60% of wall thickness, prevent freezing to ensure feeding, design specification.
Análise das causas
ABS gate size 50-60% of wall thickness; prevent premature freezing; ensure complete feeding; gate position; flow balance; sink mark prevention and control.; during on-site troubleshooting, verify item by item according to this mechanism, avoiding blind machine adjustment based solely on experience
Solução
①Gate 50-60% of wall thickness; ②position optimization; ③flow balance; ④feeding assurance; ⑤sink mark prevention and control.; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
Conclusão principal
The 50/60 rule of ABS gates is a design standard; position and size both emphasized; ensuring feeding prevents sink marks.; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
ABS; gate; 50/60 rule; wall thickness; feeding; sink mark