Material Drying 7 visualizações

ABS high-gloss part process

Fenómeno do problema
[Problem phenomenon] ABS high-gloss appearance parts have insufficient gloss or flow marks, poor paint-free effect
Análise das causas
High-gloss parts require mold temperature 75-80°C upper limit, melt temperature upper limit, and sufficient drying; any moisture or insufficient temperature manifests as gloss and flow mark defects; during on-site troubleshooting, verify item by item according to this mechanism, avoiding blind machine adjustment based solely on experience
Solução
High-gloss parts take the upper limit of mold temperature and melt temperature; stricter drying verification; cavity mirror polishing; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
Conclusão principal
ABS high-gloss parts three upper limits: mold temperature, melt temperature, drying; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for subsequent similar problems
high-gloss part mold temperature melt temperature drying