Processing Machinery 7 visualizações

ABS low-temperature toughness application

Fenómeno do problema
[Problem phenomenon] Cold-region products need low-temperature impact-resistant materials
Análise das causas
ABS low-temperature toughness is medium, cold-region applications need toughened grades or verification; low-temperature cracking starts at notches; during on-site troubleshooting, verify item by item according to this mechanism, avoiding blind machine adjustment based solely on experience
Solução
Cold-region parts select toughened ABS with low-temperature verification; structural rounding; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
Conclusão principal
ABS low temperature requires toughening verification, rounding assists; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for subsequent similar problems
low-temperature toughness cold region toughening fillet