Molds & Tooling
3 visualizações
ABS surface orange peel
Fenómeno do problema
[Problem Phenomenon] ABS high-gloss part orange-peel texture
Análise das causas
Front instability plus insufficient mold temperature; cavity transcription; during on-site troubleshooting, verify item by item according to this mechanism, avoid blindly adjusting the machine based only on experience; this mechanism has been repeatedly verified by industry materials and should be confirmed first during troubleshooting
Solução
Raise mold temperature and injection speed to stabilize front; high polishing of cavity; after adjustment, continuously sample to verify the effect, resume mass production only after confirming stability; change only one variable each time and record parameter changes to facilitate locating effective measures
Conclusão principal
ABS orange peel stabilize front plus high polishing; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems later
Isto foi útil?
0 pessoas acharam isto útil
Obrigado pelo seu comentário!