Injection Molding
5 visualizações
ASA weld line visible and low strength
Fenómeno do problema
ASA dark-colored product weld line marks are clearly visible, strength insufficient at convergence of multi-gate parts, cracks along weld line after assembly stress.
Análise das causas
When the convergence temperature of two melt fronts is insufficient, interfacial bonding is weak; ASA dark formula makes weld line visual contrast strong; Plastribution points out that high injection speed obtains the strongest weld line, low speed the opposite.
Solução
①Raise melt temperature and use the highest possible injection speed to strengthen weld line; ②raise mold temperature to 50~80℃ range; ③strengthen venting in convergence area; ④gate layout moves weld line out of appearance surface and stressed area.
Conclusão principal
ASA weld line governance counter-conventionally requires high-speed filling; weld lines on dark parts can only be relocated and are hard to eliminate; high speed must be matched with good venting.; After confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence