Molds & Tooling
3 visualizações
ASA crystallinity misunderstanding
Fenómeno do problema
[Problem phenomenon] Managing ASA process with crystalline material thinking, mold temperature and cooling logic wrong
Análise das causas
ASA is an amorphous polymer: no crystalline melting point, low shrinkage, mold temperature mainly affects surface rather than crystallinity; applying semi-crystalline management thinking leads to parameter misalignment
Solução
Set process according to amorphous logic: mold temperature serves surface, cooling serves shape setting; shrinkage compensated at 0.4-0.7%; after adjustment, continuously sample to verify the effect, and resume mass production after confirming stability
Conclusão principal
ASA is an amorphous material, mold temperature for surface cooling for shape setting; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for subsequent similar problems