Fenómeno do problema
The hardness of shoe soles varies greatly between batches in testing.
Análise das causas
Fluctuations in foaming ratio and crosslinking degree directly change the hardness; raw material batch differences are also transmitted.; During on-site troubleshooting, verify item by item according to this mechanism to avoid blindly adjusting the machine based only on experience
Solução
①Stabilize the foaming and crosslinking processes; ②test raw material batches; ③test hardness by batch; ④fix the process parameters.; After adjustment, continuously sample to verify the effect, and resume mass production after confirming stability
Conclusão principal
Hardness is a comprehensive indicator of foaming process stability; batch management is the key to control.; After confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence