Blow Molding 14 visualizações

HDPE '2079851475616104457 cooling

Fenómeno do problema
HDPE blow-molded drum deforms after demolding
Análise das causas
The thick-walled areas of the blow-molded part are insufficiently cooled, and shrinkage deformation occurs after demolding; when troubleshooting on site, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience; this mechanism has been repeatedly verified by industry data and should be confirmed first during troubleshooting
Solução
Optimize the mold cooling water circuits; sufficient blowing air cooling time; strengthen cooling at thick-walled areas; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes, to facilitate locating effective measures
Conclusão principal
Blow-molded part deformation is controlled by sufficient cooling; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar future problems
HDPE'2079851475616104457coolingdeformation