HDPE trash can

Fenómeno do problema
Outdoor trash cans embrittle and crack after a few years
Análise das causas
Outdoor UV aging embrittles HDPE, and the barrel body edges crack first; when troubleshooting on site, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience; this mechanism has been repeatedly verified by industry data and should be confirmed first during troubleshooting
Solução
Select an anti-UV carbon black grade; thicken the barrel body edges; manage according to outdoor life; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes, to facilitate locating effective measures
Conclusão principal
Outdoor trash cans must use anti-UV grades; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar future problems