LLDPE film heat sealing problem
Fenómeno do problema
Heat seal initiation temperature is high or hot tack strength is low.
Análise das causas
LLDPE has a higher melting point than LDPE, and the heat seal window is different; hot tack is related to the grade (comonomer type).
Solução
①Adjust the heat seal temperature according to the grade; ②select a heat-sealable grade (such as octene copolymer); ③optimize heat seal pressure and time; ④clean the contaminated film surface first.
Conclusão principal
For heat sealing, first check the grade's melting point and comonomer.