LLDPE film die head design matching

Fenómeno do problema
Continuing to use the LDPE die head for LLDPE production, problems occur frequently.
Análise das causas
LLDPE needs a wider die gap and dedicated flow channel design; directly applying an LDPE die head causes excessive shear.; During on-site troubleshooting, verify item by item according to this mechanism, avoiding blindly adjusting the machine based only on experience.
Solução
①Evaluate die head modification to widen the gap; ②select an LLDPE-dedicated die head; ③optimize the flow channel to reduce dead spots; ④verify the modification effect.; After adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability.
Conclusão principal
Die head matching is the hardware premise for smooth LLDPE production; a dedicated die head is a worthwhile investment.; After confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence.
LLDPE; film; die head; design; gap; modification