LLDPE mold temperature uniformity
Fenómeno do problema
LLDPE injection molded parts warpage deformation.
Análise das causas
Uneven mold cooling causes shrinkage differences; During on-site troubleshooting, verify item by item according to this mechanism, avoiding blindly adjusting the machine based only on experience; This mechanism has been repeatedly verified by industry data and should be confirmed first during troubleshooting.
Solução
Water channels equalization; cavity temperature difference ±5℃; thick-wall water channels strengthened; After adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; Change only one variable at a time and record parameter changes, to facilitate locating effective measures.
Conclusão principal
Warpage is controlled by cooling uniformity; After confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future.
Isto foi útil?
0 pessoas acharam isto útil
Obrigado pelo seu comentário!