LLDPE injection speed

Fenómeno do problema
Flash in LLDPE high-speed injection
Análise das causas
High speed and high pressure cause overflow; when troubleshooting on site, verify item by item according to this mechanism to avoid blindly adjusting the machine based only on experience; this mechanism has been repeatedly verified by industry data and should be confirmed first during troubleshooting
Solução
Speed profiling; reduce speed in final stage; clamping force calculation; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
Conclusão principal
Injection profiling prevents flash; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
LLDPEinjection speedflashprofiling