Injection Molding 2 visualizações

LLDPE '2079851475616104452 advantages

Fenómeno do problema
LLDPE injection molded parts are harder and stronger than LDPE, tougher and more stress-crack resistant than HDPE
Análise das causas
LLDPE density 0.915-0.935, tensile strength 18-22MPa, between LDPE and HDPE; elongation at break 400-700% gives excellent toughness; ESCR is extremely good, the best among the three major polyethylenes
Solução
①Choose LLDPE for stiffness-toughness balance needs; ②prefer LLDPE in stress cracking scenarios; ③select specific grades by density and melt index; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
Conclusão principal
LLDPE is the performance balance point among the three major polyethylenes; its ESCR advantage makes it irreplaceable in containers and pipes; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence