Processing Machinery
6 visualizações
LLDPE thickness band
Fenómeno do problema
Transverse thick-thin bands in LLDPE film
Análise das causas
Die lip gap deviation or airflow fluctuation; when troubleshooting on site, verify item by item according to this mechanism to avoid blindly adjusting the machine based only on experience; this mechanism has been repeatedly verified by industry data and should be confirmed first during troubleshooting
Solução
Fine die lip adjustment; automatic air ring; thickness scanning; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
Conclusão principal
Thick-thin bands rely on die lip and automatic air ring; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
Isto foi útil?
0 pessoas acharam isto útil
Obrigado pelo seu comentário!