Injection Molding 2 visualizações

PA12 Injection Pressure and Holding Pressure Strategy

Fenómeno do problema
【Problem phenomenon】PA12 products alternately showed large stress from over-holding and sink marks from insufficient compensation
Análise das causas
PA12 injection pressure can be used up to 100MPa, but low holding pressure combined with high melt temperature is recommended; high holding pressure introduces internal stress, while the crystallization volume shrinkage of semi-crystalline materials must be compensated
Solução
Set injection pressure according to flow needs with an upper limit of 100MPa; adopt a low-value long-time strategy for holding pressure; make the runner and gate dimensions large enough to compensate for crystallization shrinkage; perform stress testing on internal-stress parts
Conclusão principal
PA12 requires high-pressure filling and low holding pressure compensation, and the runner and gate must be large enough to compensate for crystallization shrinkage; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
injection pressureholding pressurecrystallization shrinkageinternal stress