Menu
Materiais Máquinas
Perspetivas
Artigos Vídeos Problema e solução
About
Sobre a Chembull Parceiros de média
Contacte-nos
Idioma
EnglishالعربيةPortuguêsEspañolDeutschTürkçe한국어
Voltar a Problema e solução
Material Drying 7 visualizações

PA6 Product Bubbles

Fenómeno do problema
Internal bubbles or surface blistering of the product, mostly occurring at thick walls, affecting appearance and strength.
Análise das causas
Moisture vaporization into bubbles is the first cause; insufficient holding pressure at thick walls forms vacuum bubbles; excessively high melt temperature decomposition also produces gas; the three mechanisms need to be distinguished (moisture is often accompanied by silver streaks, and vacuum bubbles have smooth walls).
Solução
①Strengthen drying and verify that the moisture content meets the standard with a moisture measurement method;②add holding pressure for thick-wall parts;③material temperature does not exceed the upper limit;④open or clean vent grooves at corresponding positions to ensure smooth gas discharge;⑤core-pull and reduce material at thick walls to reduce shrinkage from the source.
Conclusão principal
PA6 bubbles follow the three-way division of 'water, vacuum, decomposition': first verify drying, then look at holding pressure, and finally control temperature; moisture content of nylon material is the most common source of bubbles, and drying verification must come first.
PA6; bubbles; moisture content; vacuum bubbles; decomposition