Extrusion & Post 7 visualizações

PA66 annealing treatment application

Fenómeno do problema
Thin-walled parts molded at low mold temperature drift in dimension over time, clearance changes after assembly
Análise das causas
When mold temperature is below 40℃, PA66 thin-walled parts' crystallinity continues to change over time, dimensions unstable long-term; annealing promotes completion of crystallization, locking dimensions in a stable state
Solução
①Anneal low-mold-temperature thin-walled parts to stabilize dimensions; ②annealing temperature below the heat deflection temperature; ③slow cooling after annealing to prevent new stress; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
Conclusão principal
Annealing is dimensional insurance for low-mold-temperature PA66 parts; if high mold temperature can solve it, annealing is unnecessary, but when low mold temperature is required, annealing cannot be omitted; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence