Material Drying 7 visualizações

PCABS pre-processing verification

Fenómeno do problema
PC/ABS moisture verification <0.02% before processing, irreversible hydrolysis prevention before high temperature.
Análise das causas
Verify moisture <0.02% before PC/ABS processing; before the barrel is heated to 220-260℃; processing undried PC/ABS at high temperature triggers rapid irreversible molecular hydrolysis; the melt is already degraded before reaching the gate.
Solução
①Moisture verification before processing; ②<0.02% standard; ③confirmation before high temperature; ④awareness of irreversible hydrolysis; ⑤prevention first.; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
Conclusão principal
PCABS pre-processing verification is the key to hydrolysis prevention; irreversibility requires prevention first; standard execution ensures quality.; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
PCABS;pre-processing verification;0.02%;hydrolysis;irreversible;prevention