Fenómeno do problema
[Problem Phenomenon] PC/ABS gate cut area whitens, and the appearance surface is damaged
Análise das causas
Shear stress is concentrated in the gate area; the cut section whitens under stress; improper gate position enlarges the mark; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience
Solução
Open the gate on a non-appearance surface; trim with a sharp tool; submarine gates cut automatically; after adjustment, continuously sample to verify the effect, and resume mass production after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
Conclusão principal
PC/ABS gate marks rely on position plus sharp trimming; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems in the future
Isto foi útil?
0 pessoas acharam isto útil
Obrigado pelo seu comentário!