Fenómeno do problema
【Problem Phenomenon】PC cooling improper, demolding deformation or cycle too long
Análise das causas
PC amorphous cooling aims at shaping; insufficient cooling causes ejection deformation, excessive cooling wastes cycle; uniform mold temperature shortens cooling;During on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based solely on experience
Solução
Cooling verifies demolding rigidity according to wall thickness; uniform mold temperature; do not sacrifice quality to compress cycle;After adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability;Change only one variable at a time and record parameter changes to facilitate locating effective measures
Conclusão principal
PC cooling calculated by wall thickness, demolding rigidity has the final say;After confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence;Include this case in the defect archive as a reference for troubleshooting similar problems in the future