PC sprue material cleanliness management

Fenómeno do problema
After using regrind, product black specks increase and impact performance fluctuates, customer inspection fails
Análise das causas
Sprue material is cross-contaminated with oil, dust and other materials, and heat history causes molecular weight to decline successively; contaminated particles manifest as black specks and flow marks on transparent and light-colored parts
Solução
①Sprue material dedicated area and dedicated use, immediate crushing and sealing; ②Prohibit mixing oily material and floor-dropped material; ③Transparent parts and food-grade parts restrict or prohibit regrind;After adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
Conclusão principal
The value of regrind depends on cleanliness and heat history control; transparent and high-requirement parts should keep regrind out;After confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
PC;sprue material;black speck;contamination;food grade