Injection Molding 2 visualizações

Process Parameter Transfer Failure of PEEK

Fenómeno do problema
After a mature PEEK process is transferred from one '2079851475616104452 machine to another, defects occur frequently, identical set parameters produce vastly different quality, and the setup cycle is greatly extended.
Análise das causas
Different equipment differs in screw geometry, temperature control characteristics, and pressure transmission efficiency — nominal parameters are the same while the actual melt state differs; PEEK's narrow window amplifies the influence of inter-equipment differences.
Solução
①Re-calibrate based on the actually measured melt temperature and actual filling state; ②Record the original machine's cavity pressure curve as the transfer target; ③Re-verify key parameters on the new equipment instead of directly copying; ④Retain the first-article verification process.
Conclusão principal
The essence of PEEK process transfer is equivalent reproduction of the melt state, not copying parameters; the cavity pressure curve is the best reference for cross-equipment transfer; every piece of equipment needs independent verification.
PEEK;process transfer;equipment difference;calibration;cavity pressure;verification