Menu
Materiais Máquinas
Perspetivas
Artigos Vídeos Problema e solução
About
Sobre a Chembull Parceiros de média
Contacte-nos
Idioma
EnglishالعربيةPortuguêsEspañolDeutschTürkçe한국어
Voltar a Problema e solução
Processing Machinery 6 visualizações

PESU Electrical Properties

Fenómeno do problema
PESU high-temperature electrical insulation, stable dielectric properties.
Análise das causas
PESU volume resistivity 1.7E+15; dielectric strength 15kV/mm; dielectric constant 3.5; stable at high temperature; dissipation factor.; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based solely on experience
Solução
①Electrical performance testing; ②high-temperature verification; ③application matching; ④long-term tracking.; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record the parameter changes, to facilitate identifying effective measures
Conclusão principal
PESU electrical properties are an advantage in high-temperature applications; testing and verification ensure reliability; tracking prevents decay.; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
PESU; electrical; insulation; dielectric; high temperature; stable

Isto foi útil?

0 pessoas acharam isto útil

ChemAI