Material Drying 6 visualizações

PET sheet haze and poor transparency

Fenómeno do problema
The sheet is hazy and cloudy with reduced gloss; the appearance does not meet transparent packaging requirements
Análise das causas
Trace amounts of moisture affect PET optical properties; degraded material loses transparency; impurities from poor filtration scatter light; unstable cooling changes crystallization behavior and produces haze
Solução
① Strengthen drying performance; ② upgrade the melt filtration system; ③ optimize cooling and calendering processes to keep roll temperature stable; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
Conclusão principal
PET transparency is the product of multiple factors; any loss of control of the four variables—moisture, degradation, impurities, and crystallization—will cause haze; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
PET;sheet;haze;transparency;crystallization