Processing Machinery 6 visualizações

PLA thermal degradation yellowing

Fenómeno do problema
Products yellow and become brittle, with reduced performance.
Análise das causas
PLA has low thermal stability; excessive processing temperature or excessive residence time triggers thermal degradation; compared with traditional plastics, PLA begins to degrade at lower temperatures.; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience
Solução
① Control melt temperature at the lower limit of the 170~200℃ window; ② shorten barrel residence time; ③ lower screw speed to reduce shear heat; ④ avoid long-time shutdown with heat preservation.
Conclusão principal
PLA's thermal degradation threshold is lower than conventional plastics; low temperature and short time are the basic principles of its processing.; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
PLA;thermal degradation;yellowing;temperature;residence time;shear