Molds & Tooling 6 visualizações

PLA product ejector whitening and cracking

Fenómeno do problema
Whitening or cracking during ejection.
Análise das causas
PLA is very brittle and cracks when ejection force is concentrated; insufficient cooling results in low strength.; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience; this mechanism has been repeatedly verified by industry data and should be confirmed first during troubleshooting
Solução
① Increase ejection area; ② extend cooling; ③ balanced ejection; ④ ensure demolding draft.; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
Conclusão principal
Brittle PLA ejection requires distributed force and sufficient cooling.; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
PLA;ejector whitening;cracking;ejection;cooling;draft