Molds & Tooling 7 visualizações

POM hot runner color change

Fenómeno do problema
POM hot runner molds show color mixing for a long time after color change
Análise das causas
Old color material remains in the hot runner, and POM's flow characteristics make purging slow; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience; this mechanism has been repeatedly verified by industry data and should be confirmed first during troubleshooting
Solução
Sequence color changes from light to dark; flush the hot runner at elevated temperature; use sufficient transition material after color change; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
Conclusão principal
Color change management requires production sequencing plus sufficient flushing; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
POMhot runnercolor changeflushing