Molds & Tooling 7 visualizações

POM Short Shot Troubleshooting

Fenómeno do problema
Thin-walled parts are underfilled; after raising temperature and pressure, short shots persist and flash begins to appear
Análise das causas
For POM short shots, check feeding and equipment first: hopper bridging, check valve leakage, and unstable cushion all make the actual shot volume insufficient; poor venting also causes end underfill
Solução
①Eliminate hopper bridging and maintain a stable cushion; ②repair check valve leakage; ③increase injection rate and check venting and gate size; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
Conclusão principal
POM short shot troubleshooting goes equipment first, process second; the three checks of bridging, check valve, and cushion are the fixed opening moves; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
POM;short shot;check valve;bridging;cushion