Molds & Tooling 7 visualizações

PP Part Uneven Gloss

Fenómeno do problema
Gloss differences between areas of the same part, corresponding to mold temperature distribution.
Análise das causas
Uneven mold cooling causes different surface replication states in each area; PP crystallinity differences also manifest as gloss differences.; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience
Solução
①Balance cooling water circuits; ②measure cavity temperature distribution; ③unify mold temperature; ④repair water circuit blockages.; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
Conclusão principal
Uneven gloss points to a mold temperature distribution problem; water circuit balancing modification can solve it once and for all.; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
PP;uneven gloss;mold temperature;water circuit;crystallization;cooling