Injection Molding 7 visualizações

PPO Injection Pressure Range

Fenómeno do problema
【Problem Phenomenon】PPO filling pressure is insufficient causing short shots; after increasing pressure, flash and stress problems appear again
Análise das causas
Increasing injection pressure is beneficial for PPO melt filling of the mold, generally controlled at 100-140MPa; NPL gives a wider range of 60-150MPa; high-viscosity materials have high pressure requirements but over-pressure must be prevented
Solução
Set injection pressure within the 100-140MPa window; for short shots, prioritize raising temperature combined with raising pressure; for flash and stress parts, check clamping force and holding pressure; after adjustment, continuously sample to verify the effect, and resume mass production after confirming stability
Conclusão principal
PPO injection pressure 100-140MPa is the baseline window; raising pressure combined with raising temperature achieves balance; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence
injection pressureshort shotflashwindow