Material Drying
6 visualizações
PPO Recycling and Sustainability
Fenómeno do problema
[Problem Phenomenon] Feasibility and precautions for recycling PPO products
Análise das causas
PPO regrind can be used but must be clean to prevent contamination; drying time needs to be extended due to particle size differences, and it may affect color; the use of regrind is restricted for regulatory certified parts (drinking water, UL)
Solução
Clean the regrind and extend drying time; limit the regrind ratio for color-sensitive parts; evaluate regrind permission for certified parts according to regulations; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
Conclusão principal
PPO regrind can be used with particular care: cleanliness, drying and color are the three gates; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
Isto foi útil?
0 pessoas acharam isto útil