Molds & Tooling 7 visualizações

PPSU mold design

Fenómeno do problema
PPSU mold temperature 149~163℃ realization; heating and insulation.
Análise das causas
PPSU mold temperature 149~163℃; heating system capability; insulation plates; uniform temperature; cooling efficiency.; During on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based solely on experience
Solução
①Heating system configuration; ②insulation plate use; ③uniform temperature; ④cooling optimization; ⑤actual measurement verification.; After adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
Conclusão principal
PPSU mold high temperature is a process requirement; system design assurance; actual measurement prevents deviation.; After confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence
PPSU; mold; heating; insulation; uniform; actual measurement

Isto foi útil?