Fenómeno do problema
PP products show silver streaks and bubbles, drying is insufficient with moisture content exceeding the standard; although water absorption is low, management is still needed.
Análise das causas
PP water absorption is low but not zero; moisture vaporizes in the 200-280°C melt; 0.1% residual moisture causes silver streak surface defects; high-temperature processing amplifies the effect of trace moisture; drying management is often neglected.
Solução
①Dry at 80-90°C for 2-3 hours; ②Verify moisture content <0.1%; ③Sealed storage to prevent moisture regain; ④Strengthen management in high-humidity environments; ⑤Check drying first when troubleshooting silver streaks.
Conclusão principal
PP's low water absorption does not mean zero drying; the 0.1% red line must be quantitatively verified; high-humidity environments are risk scenarios.; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence