PP Surface Hardness Scratch
Fenómeno do problema
【Problem Phenomenon】PP product surfaces are scratched and worn
Análise das causas
PP surface hardness is low and easily scratched; obvious on high-gloss appearance parts; during on-site troubleshooting, verify item by item according to this mechanism to avoid blindly adjusting the machine based only on experience; this mechanism has been repeatedly verified by industry data and should be confirmed first during troubleshooting
Solução
Protection during transfer; surface coating; high-hardness grades or fillers; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability; change only one variable at a time and record parameter changes to facilitate locating effective measures
Conclusão principal
PP fears scratching, protective coating plus hard fillers; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems in the future
Isto foi útil?
0 pessoas acharam isto útil
Obrigado pelo seu comentário!