Extrusion & Post
14 visualizações
HIPS Sheet Extrusion Thickness Unevenness
Fenómeno do problema
The transverse thickness deviation of extruded sheets is large.
Análise das causas
Uneven die lip gap or uneven die temperature distribution; extrusion fluctuations are also transmitted.; during on-site troubleshooting, verify item by item according to this mechanism to avoid blindly adjusting the machine based only on experience; this mechanism has been repeatedly verified by industry data and should be confirmed first during troubleshooting
Solução
①Precisely adjust the die lip gap; ②balance die temperature; ③stabilize extrusion output; ④online thickness measurement feedback.; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
Conclusão principal
Sheet thickness relies on die lip precision and stable extrusion; closed-loop thickness measurement is the guarantee.; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems in the future
Isto foi útil?
0 pessoas acharam isto útil
Obrigado pelo seu comentário!