TPE Product Molding Cycle
Fenómeno do problema
Long cycle and high cost.
Análise das causas
Cooling time accounts for a large proportion; blind compression is risky.; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based solely on experience; this mechanism has been repeatedly verified by industry information and should be confirmed first during troubleshooting
Solução
①Calculate cooling according to wall thickness; ②Optimize water channels; ③Compress step by step with verification; ④Monitor quality.; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
Conclusão principal
Cycle optimization is supported by data.; after confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a reference for troubleshooting similar problems in the future
Isto foi útil?
0 pessoas acharam isto útil
Obrigado pelo seu comentário!