Fenómeno do problema
Problems occur frequently when processing TPU with the SEBS-based TPE process.
Análise das causas
TPU is more sensitive to moisture and has stricter drying requirements, otherwise it is very prone to hydrolysis producing bubbles and silver streaks; TPU is also more sensitive to shear, and excessive injection speed easily decomposes and burns.
Solução
①strictly implement drying standards for TPU; ②injection speed should not be too fast; ③set the temperature window according to TPU characteristics; ④do not copy SEBS process parameters.
Conclusão principal
The processing characteristics of TPU and SEBS-based TPE differ significantly; moisture and shear sensitivity are the two starting points of TPU process design; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence