Molds & Tooling 7 visualizações

TPU product cold slug marks

Fenómeno do problema
Cold material marks appear on the product surface.
Análise das causas
Low nozzle temperature or cold material entering the cavity; the lack of cold slug wells allows cold material to reach the product directly; during on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based only on experience
Solução
①increase nozzle temperature; ②add cold slug wells; ③optimize gate design; ④check nozzle heating; after adjustment, continuously sample to verify the effect, and resume mass production only after confirming stability
Conclusão principal
Cold slug marks rely on cold slug wells for interception; nozzle temperature management is a preventive means; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems later